yüksek sıcaklıklı nikel alaşımı
Created with Pixso.

High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners

High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners

Marka Adı: DLX
Model Numarası: GH3044 süper alaşımlı tel
Adedi: 5kg
Ödeme Koşulları: L/C,D/A,D/P,T/T,VTB
Tedarik Yeteneği: Aylık 1200 Ton
Detay Bilgisi
Menşe yeri:
Çin Jiangsu
Sertifika:
CE,ROHS
Ambalaj bilgileri:
Karton kutulu makara paketi, çoklu torbalı bobin paketi, tahta sandık paketi
Yetenek temini:
Aylık 1200 Ton
Vurgulamak:

GH3044 superalloy wire 0.5-6.0mm

,

high temp nickel alloy wire

,

superalloy wire for fasteners

Ürün Açıklaması
Solid-solution strengthened GH3044 nickel-chromium superalloy wire engineered for critical high-temperature fasteners, aerospace structural components, and high-heat springs. Manufactured through high-purity vacuum metallurgy and multi-pass precision drawing for superior thermal stability and fatigue strength. Product Overview The high-temperature fastening sector demands raw materials with flawless surface quality, uniform chemical distribution, and consistent mechanical